Internal friction in Invar Fe-35 % Ni alloy after combined SPD by hydroextrusion and drawing

Завантаження...
Ескіз

Дата

Назва журналу

Номер ISSN

Назва тому

Видавець

НТК «Інститут монокристалів» НАН України

Анотація

The temperature dependence of internal friction on frequency of ~3 Hz and ~60 Hz were studied in Invar Fe-35.0% Ni-0.49% Mn-0.03%C alloy after annealing at 1373 K and combined severe plastic deformation (SPD) by hydroextrusion and subsequent drawing with the total degree of accumulated deformation ε Σ = 4.69. The reduction of the relaxation IF peak intensity is observed in deformed sample of the alloy at ~380 K (the activation energy 0.82-0.93 eV) due to decreasing of mechanical and magnetomechanical relaxation losses the contribution of which is renewed after ageing of the deformed alloy. The damping growth nearby temperatures 780-820 K after combined SPD and partial its reduction after ageing of the alloy were revealed. The estimated activation energy of the relaxation process is 1.82-1.97 eV.

Опис

Теми

Characterization and properties

Цитування

Internal friction in Invar Fe-35 % Ni alloy after combined SPD by hydroextrusion and drawing / V.M. Nadutov, D.L. Vashchuk, A.N. Pilipenko, O.A. Davidenko, V.A. Beloshenko // Functional Materials. — 2014. — Т. 21, № 1. — С. 52-58. — Бібліогр.: 22 назв. — англ.

item.page.endorsement

item.page.review

item.page.supplemented

item.page.referenced