Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple

Завантаження...
Ескіз

Дата

Назва журналу

Номер ISSN

Назва тому

Видавець

НТК «Інститут монокристалів» НАН України

Анотація

The course of removal of oxide ion admixtures (deoxidization) from molten cesium iodide using galvanic couple zirconium-platinum at 973 K was studied by a potentiometric method using a membrane oxygen electrode Pt(O₂)⁄YSZ (YSZ - yttria stabilized zirconia) as an indicator one for the detection of current and equilibrium concentrations of O₂-. The running of the deoxidization in both cases is subjected to kinetics of 2nd order process with respect to O<m^>2- and the rate constant is as (3.07±0.31)·106 kg·mol⁻¹·min⁻¹·cm⁻² for the galvanic couple. Surface capacity of the galvanic couple with respect to oxide ions was estimated as 7.6·10-4 mol·cm⁻². The destruction and fixation of oxygen-containing admixtures in the case of the galvanic couple occur more intensively that in the case of pure zirconium and Zr-Pt combination is more promising agent for deep purification of growth halide melts.

Опис

Теми

Technology

Цитування

Study of deoxidization process of CsI melt by the action of "Zr-Pt" galvanic couple / V.L. Cherginets, T.P. Rebrova, Y.N. Datsko,A.L. Rebrov, P.V. Mateychenko // Functional Materials. — 2016. — Т. 23, № 4. — С. 644-649. — Бібліогр.: 9 назв. — англ.

item.page.endorsement

item.page.review

item.page.supplemented

item.page.referenced