Erosion properties of tungsten and WTa5 alloy exposed to repetitive QSPA plasma loads below melting threshold
dc.contributor.author | Makhlai, V.A. | |
dc.contributor.author | Herashchenko, S.S. | |
dc.contributor.author | Aksenov, N.N. | |
dc.contributor.author | Byrka, O.V. | |
dc.contributor.author | Garkusha, I.E. | |
dc.contributor.author | Malykhin, S.V. | |
dc.contributor.author | Surovitskiy, S.V. | |
dc.contributor.author | Kulik, N.V. | |
dc.contributor.author | Staltsov, V.V. | |
dc.contributor.author | Lebedev, S.I. | |
dc.contributor.author | Shevchuk, P.B. | |
dc.contributor.author | Wirtz, M. | |
dc.contributor.author | Sadowski, M.J. | |
dc.date.accessioned | 2019-02-18T19:32:15Z | |
dc.date.available | 2019-02-18T19:32:15Z | |
dc.date.issued | 2018 | |
dc.description.abstract | The damage of deformed double forged pure tungsten (W) and tungsten alloyed with 5 wt.% tantalum (WTa5) have been studied in experimental simulations of ITER-like transient events (surface heat load of 0.45 MJ/m² and the pulse duration of 0.25 ms) with quasi-stationary plasma accelerator QSPA Kh-50. The plasma exposures were performed for targets maintained at room temperature and preheated at 200 or 300°C. The large and fine cracks appeared in result of plasma impacts. The high number of repetitive plasma loads below the melting threshold led to the clear degradation of thermo-mechanical properties of the affected surface layers on tungsten. Comparative analysis of the cracks propagation to the bulk is presented for both W and WTa5 samples. | uk_UA |
dc.description.abstract | Вивчено пошкодження деформованого подвійною ковкою чистого вольфраму (W) та з легуючою 5 об.% домішкою танталу (WTa5) при експериментальному моделюванні умов перехідних процесів в ІТЕР (теплове навантаження на поверхню 0,45 МДж/м² , тривалість імпульсу 0,25 мс) у квазістаціонарному плазмовому прискорювачі КСПП Х-50. Опромінення мішеней плазмою проводили при кімнатній початковій температурі та з підігрівом до 200 та 300°C. В результаті плазмового впливу з’являлися великі й маленькі тріщини. Велика кількість повторюваних плазмових навантажень нижча порога плавлення привела до явної деградації термомеханічних властивостей пошкоджених приповерхневих шарів вольфраму. Представлено порівняльний аналіз розповсюдження тріщин в об'єм для W- і WTa5-зразків. | uk_UA |
dc.description.abstract | Изучены повреждения деформированного двойной ковкой чистого вольфрама (W) и с легирующей 5 об.% добавкой тантала (WTa5) при экспериментальном моделировании условий переходных процессов в ИТЭР (тепловая нагрузка на поверхность 0,45 МДж/м² , длительность импульса 0,25 мс) в квазистационарном плазменном ускорителе КСПУ Х-50. Облучение мишеней плазмой проводили при комнатной начальной температуре и с подогревом до 200 и 300°C. В результате плазменного воздействия появлялись большие и мелкие трещины. Большое количество повторяющихся плазменных нагрузок ниже порога плавления привело к явной деградации термомеханических свойств поврежденных приповерхностных слоев вольфрама. Представлен сравнительный анализ распространения трещин в объем для W- и WTa5-образцов. | uk_UA |
dc.description.sponsorship | This work has been carried out within the framework of the EUROfusion Consortium and has received funding from the Euratom research and training programme 2014-2018 under grant agreement No 633053. The views and opinions expressed herein do not necessarily reflect those of the European Commission. This work has been performed under EUROfusion WP PFC. This work has been also supported by the National Academy Science of Ukraine, under project X-4-3/2018 and NMRT-2/2018. | uk_UA |
dc.identifier.citation | Erosion properties of tungsten and WTa5 alloy exposed to repetitive QSPA plasma loads below melting threshold / V.A. Makhlai, S.S. Herashchenko, N.N. Aksenov, O.V. Byrka, I.E. Garkusha, S.V. Malykhin, S.V. Surovitskiy, N.V. Kulik, V.V. Staltsov, S.I. Lebedev, P.B. Shevchuk,M. Wirtz, M.J. Sadowski // Вопросы атомной науки и техники. — 2018. — № 6. — С. 59-62. — Бібліогр.: 15 назв. — англ. | uk_UA |
dc.identifier.issn | 1562-6016 | |
dc.identifier.other | PACS: 52.40.HF | |
dc.identifier.uri | https://nasplib.isofts.kiev.ua/handle/123456789/148819 | |
dc.language.iso | en | uk_UA |
dc.publisher | Національний науковий центр «Харківський фізико-технічний інститут» НАН України | uk_UA |
dc.relation.ispartof | Вопросы атомной науки и техники | |
dc.status | published earlier | uk_UA |
dc.subject | ИТЭР и приложения для термоядерного реактора | uk_UA |
dc.title | Erosion properties of tungsten and WTa5 alloy exposed to repetitive QSPA plasma loads below melting threshold | uk_UA |
dc.title.alternative | Особливості ерозії вольфраму та сплаву WTa5, опромінених повторювальними плазмовими навантаженнями КСПП нижче порога плавлення | uk_UA |
dc.title.alternative | Особенности эрозии вольфрама и сплава WTa5, облученных повторяющимися плазменными нагрузками КСПУ ниже порога плавления | uk_UA |
dc.type | Article | uk_UA |
Файли
Оригінальний контейнер
1 - 1 з 1
Завантаження...
- Назва:
- 15-Makhlai.pdf
- Розмір:
- 830.11 KB
- Формат:
- Adobe Portable Document Format
Контейнер ліцензії
1 - 1 з 1
Завантаження...
- Назва:
- license.txt
- Розмір:
- 817 B
- Формат:
- Item-specific license agreed upon to submission
- Опис: