Failure of Zr50 Ti16.5 Cu15 Ni18.5 amorphous metallic ribbon
dc.contributor.author | Miskuf, J. | |
dc.contributor.author | Csach, K. | |
dc.contributor.author | Jurikova, A. | |
dc.contributor.author | Ocelik, V. | |
dc.contributor.author | Bengus, V. | |
dc.contributor.author | Tabachnikova, E. | |
dc.date.accessioned | 2013-08-19T12:47:12Z | |
dc.date.available | 2013-08-19T12:47:12Z | |
dc.date.issued | 2008 | |
dc.description.abstract | The deformation and fracture behavior of Zr50Ti165Cu15Ni185 bulk amorphous metal in the form of a thin ribbon have been determined in tensile test at room temperature. The fracture is localized in a major shear band and the fracture angle between the tensile stress axis and the fracture plane is close to 45°. Fractographic observations have revealed that the fracture surface of the amorphous metallic glass consists mainly of a vein-like pattern morphology We present a scheme of three zones of fracture surface morphology: progressive smooth sliding region (A), dominating vein like pattern (B), and river-like ripples (C). | uk_UA |
dc.description.abstract | Исследованы особенности деформирования и разрушения массивного аморфного металла 2г50Т116.5Си15№185 в виде тонкой ленты при испытании на растяжение при комнатной температуре. Разрушение локализуется в главной полосе сдвига, при этом угол разрушения между осью растягивающего напряжения и плоскостью разрушения близок к 45°. Фрактографические исследования показали, что поверхность излома аморфного металлического стекла состоит в основном из жильной морфологии. Приведена схема трех зон морфологии поверхности излома: область последовательного непрерывного скольжения (А), преобладающая жильная структура (В) и “речная” рябь (С). | uk_UA |
dc.description.sponsorship | This work was supported by the Slovak Grant Agency for Science - VEGA. | uk_UA |
dc.identifier.citation | Failure of Zr50 Ti16.5 Cu15 Ni18.5 amorphous metallic ribbon / J. Miskuf, K. Csach, A. Jurikova, V. Ocelfk, V. Bengus, E. Tabachnikova // Проблемы прочности. — 2008. — № 1. — С. 28-31. — Бібліогр.: 15 назв. — англ. | uk_UA |
dc.identifier.issn | 0556-171X | |
dc.identifier.udc | 539. 4 | |
dc.identifier.uri | https://nasplib.isofts.kiev.ua/handle/123456789/48411 | |
dc.language.iso | en | uk_UA |
dc.publisher | Інститут проблем міцності ім. Г.С. Писаренко НАН України | uk_UA |
dc.relation.ispartof | Проблемы прочности | |
dc.status | published earlier | uk_UA |
dc.subject | Научно-технический раздел | uk_UA |
dc.title | Failure of Zr50 Ti16.5 Cu15 Ni18.5 amorphous metallic ribbon | uk_UA |
dc.title.alternative | Разрушение аморфной металлической ленты из Zr5o Tii6.5 Cui5 Nii8.5 | uk_UA |
dc.type | Article | uk_UA |
Файли
Оригінальний контейнер
1 - 1 з 1
Контейнер ліцензії
1 - 1 з 1
Завантаження...
- Назва:
- license.txt
- Розмір:
- 817 B
- Формат:
- Item-specific license agreed upon to submission
- Опис: