Paramagnetic defects related to photoluminescence in SiOx films

dc.contributor.authorRudko, G.Yu.
dc.contributor.authorVorona, I.P.
dc.contributor.authorIndutnyy, I.Z.
dc.contributor.authorIshchenko, S.S.
dc.contributor.authorShepeliavyi, P.E.
dc.contributor.authorYukhymchuk, V.O.
dc.date.accessioned2017-06-05T09:24:14Z
dc.date.available2017-06-05T09:24:14Z
dc.date.issued2004
dc.description.abstractThe correlation between the photoluminescence and paramagnetic defects is studied in SiOx films grown by vacuum thermal deposition and annealed at 750 ⁰C. The as-grown samples exhibit a wide structureless EPR line centered at g = 2.0040, which is explained by the presence of a variety of dangling bonds •Si = SiyO₃–y. The annealing at 750 ⁰C causes the formation of amorphous silicon inclusions in SiOx matrix, appearance of the photoluminescence peaked at ~ 1.8 eV and shift of the EPR line to the low field range. The latter implies the preferable annealing of the paramagnetic defects in the regions of the sample with higher concentration of oxygen. The optically detected magnetic resonance studies show that these defects are not responsible for the luminescence; they are the centers of nonradiative recombination, but the efficiency of photoluminescence quenching due to these defects is rather low.uk_UA
dc.description.sponsorshipThe authors are grateful to Prof. W.M. Chen and Prof. I.A. Buyanova for the possibility to carry out the ODMR experiments. This study was funded by the Programs of the National Academy of Sciences of Ukraine “Optical and spectroscopic investigations of semiconductors and semiconductor structures” and “Magnetic resonance and optical study of defects in semiconductors and dielectrics”.uk_UA
dc.identifier.citationParamagnetic defects related to photoluminescence in SiOx films / G.Yu. Rudko, I.P. Vorona, I.Z. Indutnyy, S.S. Ishchenko, P.E. Shepeliavyi, V.O. Yukhymchuk // Semiconductor Physics Quantum Electronics & Optoelectronics. — 2004. — Т. 7, № 4. — С. 400-403. — Бібліогр.: 9 назв. — англ.uk_UA
dc.identifier.issn1560-8034
dc.identifier.otherPACS: 76.70.Hb, 78.55.Hx, 78.66.Sq
dc.identifier.urihttps://nasplib.isofts.kiev.ua/handle/123456789/119207
dc.language.isoenuk_UA
dc.publisherІнститут фізики напівпровідників імені В.Є. Лашкарьова НАН Україниuk_UA
dc.relation.ispartofSemiconductor Physics Quantum Electronics & Optoelectronics
dc.statuspublished earlieruk_UA
dc.titleParamagnetic defects related to photoluminescence in SiOx filmsuk_UA
dc.typeArticleuk_UA

Файли

Оригінальний контейнер

Зараз показуємо 1 - 1 з 1
Завантаження...
Ескіз
Назва:
15-Rudko.pdf
Розмір:
171.77 KB
Формат:
Adobe Portable Document Format

Контейнер ліцензії

Зараз показуємо 1 - 1 з 1
Завантаження...
Ескіз
Назва:
license.txt
Розмір:
817 B
Формат:
Item-specific license agreed upon to submission
Опис: